Cold polymerizing acrylic material for the manufacturing of hard, fadeless earmolds. Free of amine and cadmium. Polymerization under pressure at a minimum of 2 bar and a maximum of 6 bar and at a temperature of 40 - 45 °C (104 - 113 °F). Polymerization time: 12 minutes.
egger Acryl/B Monomer (liquid), 250 ml
Polymerization time: 12 min.
Color: transparent
Storage Temperature <30°C
Contents: 250 ml