Colored, opaque cold polymerizing acrylic material for the manufacturing of hard, fadeless earmolds. Free of amine and cadmium. Polymerization under pressure at a minimum of 2 bar and a maximum of 6 bar and at a temperature of 40 - 45 °C (104 - 113 °F). Polymerization time: 12 minutes.
egger Acryl/B Polymer (powder), white, 200 g
Mixing ratio: Monomer : Polymer = 1 : 2
Storage Temperature <30°C
Color: white
Contents: 0,2 kg
Documents for download
Process description (Login required)