Hot polymerizing acrylic material for the manufacturing of soft, with body temperature smooth acrylic earmolds for the microwave technique. Combined earmolds (soft auditory canal, hard concha) possible by combining with Fricotherm. Polymerization at 7 bar pressure in Micropol 2000. Polymerization time: 10 minutes.
Varioflex-Liquid II (Monomer), transparent, 1 l